Electrochemical Shear Thickening Polishing (ESTP) Technology for Single Crystal SiC +

Electrochemical Shear Thickening Polishing (ESTP) Technology for Single Crystal SiC +

PAM-XIAMEN can offer 4H-SiC and 3C-SiC substrates, more info please contact at [email protected]. Single crystal silicon carbide (4H-SiC), as a wide bandgap semiconductor material, has important application prospects in high-frequency, high-temperature, and high-power devices. However, its high hardness, brittleness, and chemical inertness make it difficult for traditional polishing to achieve high material removal rates and non-destructive ultra smooth surfaces simultaneously. Electrochemical Shear Thickening Polishing (ESTP) effectively solves this problem by combining anodizing with Shear Thickening Polishing (STP). This article provides a systematic overview of the mechanism of action of ESTP, optimization strategies for key process parameters such as voltage, electrolyte, and abrasive properties, as well as its effectiveness in removing surface/subsurface damage (SSD).

1. Principle of ESTP Technology

The ESTP system, as shown in Fig. 1, consists of two core units: electrochemical anodizing and shear thickening polishing. The workpiece (anode) and the graphite electrode (cathode) in the polishing tank form a closed electrolytic circuit, and the following reactions occur in the electrolyte (such as NaNO3):

Cathodic reaction: 2H2O+2e − → H2 ↑+2OH −

Anodic reaction: SiC+4OH − 8e − → SiO2+CO2 ↑+4H+

Fig. 1 (a) Working principle of electrochemical shear thickening polishing; (b) Microscopic material removal process of ESTP

Fig. 1 (a) Working principle of electrochemical shear thickening polishing; (b) Microscopic material removal process of ESTP

The hardness of the generated SiO2 layer significantly decreased (from 21.07 GPa to 0.96 GPa), followed by shear thickening of STF under high-speed rotation, driving efficient removal of the oxide layer by CeO2/diamond abrasive clusters. Through the dynamic equilibrium of oxidation removal, continuous material removal and surface leveling are achieved.

2. Influence and Optimization of Key Parameters in ESTP

2.1 Control Mechanism of Anodizing Process

Hang et al. (2025) found through TEM/EDS analysis that surface damage (such as microcracks and dislocations) on the original workpiece significantly affects the uniformity of the oxide layer: the oxidation rate in the damaged area is higher than that in the undamaged area, leading to the protrusion and delamination of the oxide layer.

Fig.2 Observation of 4H-SiC substrate after anodizing for 5 minutes

Fig.2 Observation of 4H-SiC substrate after anodizing for 5 minutes: (a) Cross sectional bright field TEM image; (b) (d) and (j) are enlarged images of the marked area in (a); (c) EDS scan shows the O in (b); high-resolution transmission electron microscopy images of the marked areas in (e) and (d); (f) EDS scan of O in (d); (g) EDS scan of Si in (d); (h) FFT results for the regions shown in (i) and (e); (k) O in EDS scan (j)

Extending the oxidation time (30 min) or increasing the voltage (20 V) can cause cracking of the oxide layer, but the substrate is not damaged. The type of electrolyte directly affects the physicochemical properties of the oxide layer:

KOH electrolyte: Strong activation ability, high current density, but there are point like protrusions in the oxide layer and a lot of Si-C bond residue (XPS results), indicating incomplete oxidation;  

NaNO3 electrolyte: generates a uniform flocculent oxide layer, with complete disappearance of Si-C bonds and the most complete oxidation;  

CA electrolyte: The oxide layer appears as granular protrusions with low hardness.  

Nanoindentation testing showed that the elastic modulus and hardness of the oxide layer formed by NaNO3 electrolyte best matched the polishing requirements and were determined to be the optimal choice.

2.2 Voltage and Oxidation Removal Balance

Shen et al. (2024) found that voltage is the key to controlling the oxidation rate. Under low voltage (3V), the polishing rate is greater than the oxidation rate, resulting in direct scratching and scratching of the substrate; If the voltage is too high (10 V), the oxidation rate will be greater than the polishing rate, and the residual oxide layer will reduce the surface quality. By calculating the charge transfer amount using Faraday’s law of electrolysis, the optimal voltage was determined to be 6V (charge transfer rate 15.70 C/min), at which the oxidation and removal rates were balanced. The MRR reached 255.5 nm/min, and the Sa decreased to 1.4nm. Subsequent research will further increase the optimized voltage to 10 V and the MRR to 321.7 nm/min.

2.3 Optimization of Abrasive Parameters and Rheological Properties

Shen et al. (2025) found through rheological testing that abrasive concentration and size significantly affect the shear thickening performance of STF:

Concentration effect: When the concentration is ≥12 wt%, the thickening effect of STF weakens or even disappears due to excessive particle damage to the force chain structure; The optimal concentration is 9 wt%;  

Size influence: Although small-sized abrasives (such as # 13000) increase the number of particles per unit volume, they lead to an increase in initial viscosity and a decrease in thickening ratio (k value); #8000 abrasives achieve the best balance between thickening effect and removal efficiency;  

Proportional effect: CeO2 is mainly used for chemical removal of SiO2 (via reaction: CeO2+H2O → Ce (OH) 2, which then reacts with Si (OH) 2 to form CeSiO4), while diamond is responsible for mechanical removal. The MRR is highest when the ratio is 4:1 (CeO2: diamond).  

Orthogonal experimental range analysis shows that abrasive concentration has the greatest impact on MRR and Sa (contribution 35.4-51.0%), followed by abrasive ratio (31.6-34.2%).

3. ESTP Effect and Damage Removal Mechanism

3.1 Elimination of Surface and Subsurface Damage

TEM cross-sectional analysis shows that there are dislocations, microcracks, and amorphous layers on the original surface of the 4H SiC substrate. After ESTP polishing (30min, 10V), the SSD was completely removed, and the FFT diffraction spots showed clear lattice structure, confirming the acquisition of a non-destructive 4H-SiC surface. When treated separately with STP, the MRR was only 123.6nm/min, and SSD removal was not thorough, confirming the critical role of electrochemical oxidation.

Fig. 3 Surface morphology of 4H-SiC substrate smoothed and polished using ESTP

Fig. 3 Surface morphology of 4H-SiC substrate smoothed and polished using ESTP

3.2 Transformation of Material Deformation Behavior

Nano scratch and indentation tests indicate that anodizing transforms SiC from brittle fracture to plastic deformation:

Before oxidation: transverse cracks and brittle fractures appear around the scratch;  

After oxidation: only plastic flow chips are seen, no cracks are generated.  

This transformation is attributed to the soft nature of the SiO2 layer, which makes it easier to achieve plastic domain removal during abrasive action.

These results indicate that ESTP technology has significant advantages and application potential in the polishing of 4H-SiC.

Whether you need 4H-SiC wafer for research or for industrial applications, please contact us email at [email protected] and [email protected].

 

References:

  1. Shen, M., Wu, L., Wei, M., Chen, H., Yuan, J., Lyu, B., … & Hang, W. (2024). High-efficiency free-damage electrochemical shear-thickening polishing of single-crystal silicon carbide. Journal of Manufacturing Processes, 132, 532-543.
  2. Hang, W., Shen, M., Wei, M., Wu, L., Wang, Y., Chen, H., … & Zhao, J. (2025). Electrochemical shear-thickening polishing of 4H-SiC (000-1): Factors influencing the anodization process. Ceramics International.
  3. Shen, M., Wei, M., Wu, L., Han, Y., Hong, B., Lyu, B., … & Hang, W. (2025). Dominant parameters and mechanisms influencing the electrochemical shear-thickening polishing of 4H-SiC. Ceramics International, 51(8), 10351-10364.