Comparative Study on Polishing Characteristics of C-face and Si-face of 4H-SiC Wafers +
PAM-XIAMEN can supply single-side or double-side chemically mechanically polished 4H-SiC wafers for epitaxial growth. For more technical parameters, please contact [email protected].
Silicon Carbide (SiC), as a third-generation wide-bandgap semiconductor material, has been widely applied in high-temperature, high-frequency, and high-power devices due to its excellent properties such as high hardness, high thermal conductivity, and good chemical stability. Single-crystal 4H-SiC is one of the most commonly used polytypes. Its crystal structure exhibits hexagonal symmetry along the [0001] direction, giving rise to two polar-opposite crystal faces: the C-face (000-1) and the Si-face (0001). Owing to differences in atomic arrangement, chemical bonding, and mechanical properties between these two faces, their material removal behaviors during machining and polishing processes differ significantly. This article reviews the performance of the C-face and Si-face in nano-scratch tests, double-sided mechanical polishing (MP), and femtosecond laser-assisted chemical mechanical polishing (CMP). It aims to reveal the intrinsic mechanisms behind their distinct polishing characteristics, thereby providing theoretical guidance for the high-efficiency and low-damage ultraprecision machining of SiC.
1. Fundamental Differences between C-face and Si-face of Single-Crystal SiC
From a crystallographic perspective, the C-face is terminated by carbon atoms, whereas the Si-face is terminated by silicon atoms. Their differing atomic configurations and surface energies lead to significant distinctions in mechanical properties and machining responses. Through nano-scratch tests, Tang et al. found that the Si-face exhibits superior stability and ductile removal capability. Their study indicates that the critical depth for the brittle-to-ductile transition is approximately 105.5nm for the Si-face, compared to about 212.3nm for the C-face, suggesting that brittle fracture initiates earlier and damage is more severe on the C-face. This disparity may be related to the elemental types and mechanical properties of the two faces. Furthermore, as shown in Fig. 1, the distinct microstructure of the Si- and C-faces directly influences their material removal mechanisms during polishing.
Fig. 1 Schematic diagram of the microstructure of the Si-face and C-face of single-crystal 4H-SiC
2. Material Removal Behavior of C-face and Si-face of 4H-SiC during Mechanical Polishing
In double-sided mechanical polishing (MP), the surface quality and material removal rate (MRR) of the C-face and Si-face show systematic differences. Zhang et al. systematically investigated the influence of polishing parameters on MRR by establishing a kinematic model and conducting orthogonal experiments. Their research found that under the optimal parameter combination (m=-1, n=5, RB=75), the maximum MRR of the SiC substrate can reach 2.7μm/h. After MP processing, the surface roughness (Ra) of the Si-face ranges from -4.9nm to 4.4nm (over a 10μm×10μm area), while that of the C-face ranges from -6.7nm to 7.8nm, indicating that a smoother surface can be achieved on the Si-face. SEM images clearly show that the post-polish Si-face surface is more uniform with fewer defects; AFM images further confirm the superior flatness of the Si-face at the nanoscale.
Fig. 2 Comparison of SEM surface morphology of (a) C-face and (b) Si-face after mechanical polishing (Magnification: 10000×)
Fig. 3 AFM surface roughness analysis results of C-face and Si-face after mechanical polishing (Scan area: 10μm×10μm)
3. Differences in Brittleness and Crack Propagation of C-face and Si-face in Nano Scratch Tests
Nano-scratch testing is a crucial method for studying material removal mechanisms at the micro-scale. Through single/double varied-load nano scratch experiments, researchers such as Tang et al. systematically compared the differences between the C-face and Si-face in terms of crack formation, propagation, and material fracture. The results indicate that the scratching process on the Si-face is more stable, with brittle removal occurring later. In contrast, the scratch path on the C-face is prone to deflection, its depth-distance curve exhibits greater fluctuation, and brittle damage is more severe. Furthermore, in double-scratch tests with varying intervals, the degree of crack interaction between scratches on both faces weakens as the interval increases, providing a basis for optimizing abrasive distribution in actual grinding and polishing processes.
4. Response Differences of the C- and Si-Faces in Femtosecond Laser-Assisted Polishing
Femtosecond laser irradiation is an effective surface modification technique that can significantly enhance CMP efficiency. According to research by Zhang et al., the ablation threshold of the C-face is lower than that of the Si-face, and under the same laser fluence, the modification line width on the C-face is larger. However, after laser irradiation, the nanoindentation hardness of the modified layer on the C-face is higher than that on the Si-face. In the subsequent CMP process, laser irradiation increased the MRR of the C-face by 77% and the Si-face by 207%, demonstrating that the laser-induced periodic surface structures significantly promote material removal. Raman spectroscopy analysis also indicates graphitization occurs on the surfaces of both faces after laser irradiation.
Fig. 4 SEM images of the femtosecond laser-irradiated (a-c) C-face and (d-f) Si-face, including top view, 52° tilt view, and cross-sectional view
Fig. 5 Nanoindentation load-displacement curves of the (a) C-face and (b) Si-face after femtosecond laser irradiation
In summary, the differences in polishing performance between the C-face and Si-face of 4H-SiC primarily stem from their surface atomic configurations, chemical bond strengths, and mechanical anisotropy. The superior performance of the Si-face in mechanical polishing is related to its larger ductile region and lower tendency for brittle damage. While the C-face has a lower ablation threshold in laser-assisted polishing, its modified layer exhibits higher hardness, reflecting the different responses of the two faces under thermo-mechanical coupling. In practical ultraprecision machining, if high surface quality and stability are the primary goals, the Si-face should be prioritized for processing. If energy-assisted methods like lasers are employed, a balance between the removal efficiency and surface integrity of both faces must be considered based on the specific process objectives.
Whether you need SiC substrate for research or for industrial applications, please contact us email at [email protected] and [email protected].
References:
- Tang, K., Ou, W., Mao, C., Liang, J., Zhang, M., Zhang, M., & Hu, Y. (2023). Material removal characteristics of single-crystal 4H-SiC based on varied-load nanoscratch tests. Chinese Journal of Mechanical Engineering, 36(1), 111.
- Zhang, P., Yang, J., & Qiu, H. (2022). Material removal rate of double-faced mechanical polishing of 4H-SiC substrate. The International Journal of Advanced Manufacturing Technology, 118(11), 3983-3993.
- Chen, Y. D., Liu, H. Y., Cheng, C. Y., & Chen, C. C. (2022). Comparison of C face (000 1¯) and Si face (0001) of silicon carbide wafers in femtosecond laser irradiation assisted chemical–mechanical polishing process. Applied Physics A, 128(12), 1094.